Customization: | Available |
---|---|
Material: | Organic Silicone |
Application: | Medical, Industrial |
Still deciding? Get samples of $ !
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() |
---|---|
Support payments in USD |
Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Pad Printing silicone | ||||||||||
Item | Mixing Ratio | Color | Hardness(shore A) | Viscosity (mPa.s) | Working Time (25ºC) | Curing Time (25ºC) | Tear-Strength (kN/m) | Tensile- Strength (Mpa) | Elongation (%) | Shrinkage(%) |
OTT-Y230 | 9:1 | red/white | 30±2 | 6000±2000 | 10-30mins | 1-5h | ≥25 | ≥5 | ≥400 | ≤0.1 |
OTT-Y235 | 9:1 | red/white | 35±2 | 7000±2000 | 10-30mins | 1-5h | ≥18 | ≥5 | ≥400 | ≤0.1 |
(1)If the silicon pad is too hard while the pattern is very delicate or small, the printing patterns will be incomplete or not very clear, for in that way the silicon pad could not adsorb the printing ink from the steel plate well. If your pattern is very delicate or small, please use soft silicon pad for pad printing.
(2)If the percentage of water in the ink is very high, the printing pattern also will be incomplete, and spot may appeared. For this situation, please clean your ink box, or change the printing ink or Tianna water.
The reasons why the silicone pad has a short service life are listed as follows:
(1)The problem caused by inappropriate filtration of silicone rubber, and impurities in the packaging process due to the uncleanness of barrels and bags.
(2)The short service life of the silicone pad has a close relationship with the adding amount of silicone oil. The more the silicone oil added, the softer the silicone pad will be. The silicone oil will destroy the molecule of the silicone rubber, thereby bringing about the non-durable and easy aging of the silicone pad.
(3)All the users should know the properties of pad printing silicone rubber. The service life of the silicone pad has close relationship with the size of the printed patterns. For example, if a big pattern to be printed, a big silicone pad is required; if a small pattern to be printed, a small silicone pad (the silicone pad has to be adjusted according to the size of the patterns, and the proportion between the size of the silicone pad and the pattern is 3:1.)
Why RTV-2 room temperature silicone rubber for elastic silicone rubber pad /printing pad silicone?
(1)If the silicon pad is too hard while the pattern is very delicate or small, the printing patterns will be incomplete or not very clear, for in that way the silicon pad could not adsorb the printing ink from the steel plate well. If your pattern is very delicate or small, please use soft silicon pad for pad printing.
(2)If the percentage of water in the ink is very high, the printing pattern also will be incomplete, and spot may appeared. For this situation, please clean your ink box, or change the printing ink or Tianna water.
1. What's silicone products you are making?
--liquid silicone, silicone rubber, silicone oil; Due to different silicone molds, our silicone has different viscosity, and cause different hardness, density to meet the requests from client.
2. Do you offer free sample to client?
--Yes, we can provide the sample for test.
3. How about the quality control in your factory?
--We have professional QC team to control the quality during production. Goods will be 100% inspected before shipment.
4. How to remove the bubbles during my mould making?
--After mixing liquid silicone with curing agent, please put the material into vacuum machine to take off the bubbles.
5. How to get good silicone mould to use longer time?
--The best way is: #A, Please choose the right liquid silicone according to your products. #B, Don't use any silicone oil in mold making, because it can make the silicone mould become too soft to use. #C, Silicone mould can be used longer after the whole silicone mould fully cured, so it's better to wait 2 hours after mould finished.
6. Why silicone rubber add curing agent after mixing a lot of bubbles?
--This is normal physical phenomena. The liquid will produce a large number of bubbles in the mixing time, so, it must pass through the vacuum exhaust bubble treatment.